Lever Arm Creep Testing Machines

The Kappa LA lever-arm creep testing machine is designed for creep tests over 10,000 hours.
Creep LA header
Kappa LA dead weight

Kappa LA with Dead Weight

This Kappa LA lever arm testing machine maintains constant load application via the gravity force of the dead weights and the patented lever arm.

  • Wear-free flexible joints provide high-quality lever arm mounting and ensure Class 1 measurement accuracy in a measurement range from 1 to 100% of nominal force as per ISO 7500-2.
  • No friction, no wear and constant force application.
  • Maximum precision, maximum reliability and long service life
  • Controlled lead screw drive maintains the lever-arm in a horizontal position during the test
  • Axiality compensating links in the load axis
Kappa LA

Kappa LA with Pretensioned Spring

This Kappa LA lever arm testing machine maintains constant load application via a pretensioned spring and the patented lever arm mounting.

  • Wear-free flexible joints provide high-quality lever arm mounting and ensure Class 1 measurement accuracy in a measurement range from 1–100% of nominal force as per ISO 7500-2, while eliminating knife-edge problems during the entire service life of the machine.
  • No friction, no wear, and constant force application
  • Maximum precision, maximum reliability and a long service life
  • Precise load and strain control
  • Controlled lead screw drive maintains the lever arm in a horizontal position during the test
  • Axiality compensating links in the load axis

Vallourec equips research center with 60 ZwickRoell creep testing machines

The Vallourec group is the leading manufacturer of seamless hot-rolled steel tubes, with manufacturing plants in Europe, Brazil, the USA and China. The new Vallourec research center in Riesa (Germany) employs experts in the fields of metallurgy, materials testing, steam oxidation, and product simulation. The experts have access to state-of-the-art technical equipment, comprising amongst others a scanning electron microscope and, at present, 26 Messphysik Kappa 50 LA creep testing machines. In mid-2013 the laboratory has been extended by further 34 additional lever-arm creep testing machines.
DSCF0206_edited
Accessories

Accessories

If you require maximum precision and reliability, the Kappa series of creep testing machines is for you. The following accessories are also available:

  • High-temperature furnaces for metals (temperature range +100/200°C to 1,200°C)
  • High-temperature furnaces for ceramics (up to 1,600°C)
  • Temperature chambers (temperature range -80°C to + 280°C/optional +350°C)
  • Temperature controller
  • Mechanical high-temperature extensometer with axial or horizontal sensors
  • Optical high-temperature extensometer with laser speckle technology
  • High-temperature load string for electromechanical and lever arm creep testing machines
  • Electronics and testXpert software: This easy-to-use system is equipped with state-of-the-art technology and based on a versatile modular concept, guaranteeing maximum data security. The large number of test program types allow the requirements of a wide range of standards, applications, and test types to be accommodated.

High-temperature adapter:

  • Standard adapter for threaded specimens in metric and Imperial/US dimensions
  • Standard adapter for flat specimens and pipe section specimens
  • Standard adapter for CT specimens to ASTM E1457 for crack propagation creep tests
Top